Quick search
Products
- Articles coming soon
- Articles coming soon
Raw Materials
Processes
- Binding
- Collating
- Corner cutting
- Creasing
- Cutting
- Cutting to size
- Die-cutting
- Edge painting
- Flocking
- Foil stamping
- Folding
- Gluing
- Grommeting
- Hole drilling
- Hole punching
- Hot Stamping
- Laminating
- Numbering
- Padding
- Perfect binding
- Perforating
- Round cornering
- Saddle stitching
- Sealing
- Spiral binding
- Stapling
- Tabbing
- Show Remaining Articles (8) Collapse Articles
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
Operations
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Blistering or cockling
- Blowing in dryers
- Breaks, dryer section
- Build-up on dryers
- Curl in paper
- Cutting in dryers
- Dimensional stability
- Dryer area defects
- Dryer felts
- Dryer temperature control
- Dryer wraps
- Drying uniformity
- Evaporation rate, maintaining
- Felt tension control
- Hot dryer bearings
- Moisture streaks in dryers
- Over-drying
- Shrinkage control
- Uneven drying
- Air in the system
- Blotches in the sheet
- Breaks, wet end
- Crush
- Dirt in the sheet
- Drainage varying
- Grainy edges, reduction
- Holes in the sheet
- Pinholes, reducing
- Sheet sealing
- Stock jumping
- Stock skating on wire
- Stock sticking to wire
- Strings, elimination
- Watermarking with ring
- Wet/dry line moving
- Wire marks
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Breaks, press section
- Bulk improvement
- Crushing, press
- Leaking doctor blades
- Moisture profile
- Peeling, press rolls
- Pickup problems
- Pitch on doctor blades
- Press cuts/wrinkles
- Press picks
- Rewet problems
- Shadow marking
- Sheet blowing, press nips
- Sheet crushing
- Sheet following top press rolls
- Sheet stealing
- Vibration at press
- Water removal (CD)
- Water removal, wet press
- Wrinkles, press section
- Show Remaining Articles (1) Collapse Articles
- Annular rings
- Baggy rolls
- Bursting or cracked rolls
- Cleaner slitting
- Corrugations
- Corrugations, winders
- Defective splices
- Dust in rolls
- Dust in the rolls
- Good roll condition, off winder
- Hard and soft spots/ridges
- Interweaving
- Loose cores
- Loose paper, in roll
- Nicked edges
- Out-of-round rolls
- Reel or roll quality
- Rewound roll quality
- Run-in of slit rolls
- Shipping roll characteristics
- Snap-offs
- Soft edges
- Starred rolls
- Telescoping
- Turned edges
- Variable density rolls
- Winder cracks
- Winding requirements
- Wrinkles, winder
- Show Remaining Articles (10) Collapse Articles
Careers
Pulp & Paper Manufacturing
- Articles coming soon
Companies
Table of Contents
1. This is caused by:
— varying web tension as the roll is being wound.
— changing pressure or speed of the riding roll when winding.
— variation in the relative torque of the two winding drums giving different densities from the core to the outside face.
2. May be corrected by rewinding with a constant-tension device.
3. Adjust the winding drums so the difference in torque is gradually reduced as the roll is built.
4. Ensure that the speed of the riding roll is reduced at a rate that it compensates for the pressure on the drums generated by the increasing weight of the windup reel as it builds.