Quick search
Products
- Articles coming soon
- Articles coming soon
Raw Materials
Processes
- Binding
- Collating
- Corner cutting
- Creasing
- Cutting
- Cutting to size
- Die-cutting
- Edge painting
- Flocking
- Foil stamping
- Folding
- Gluing
- Grommeting
- Hole drilling
- Hole punching
- Hot Stamping
- Laminating
- Numbering
- Padding
- Perfect binding
- Perforating
- Round cornering
- Saddle stitching
- Sealing
- Spiral binding
- Stapling
- Tabbing
- Show Remaining Articles (8) Collapse Articles
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
Operations
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Blistering or cockling
- Blowing in dryers
- Breaks, dryer section
- Build-up on dryers
- Curl in paper
- Cutting in dryers
- Dimensional stability
- Dryer area defects
- Dryer felts
- Dryer temperature control
- Dryer wraps
- Drying uniformity
- Evaporation rate, maintaining
- Felt tension control
- Hot dryer bearings
- Moisture streaks in dryers
- Over-drying
- Shrinkage control
- Uneven drying
- Air in the system
- Blotches in the sheet
- Breaks, wet end
- Crush
- Dirt in the sheet
- Drainage varying
- Grainy edges, reduction
- Holes in the sheet
- Pinholes, reducing
- Sheet sealing
- Stock jumping
- Stock skating on wire
- Stock sticking to wire
- Strings, elimination
- Watermarking with ring
- Wet/dry line moving
- Wire marks
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Articles coming soon
- Breaks, press section
- Bulk improvement
- Crushing, press
- Leaking doctor blades
- Moisture profile
- Peeling, press rolls
- Pickup problems
- Pitch on doctor blades
- Press cuts/wrinkles
- Press picks
- Rewet problems
- Shadow marking
- Sheet blowing, press nips
- Sheet crushing
- Sheet following top press rolls
- Sheet stealing
- Vibration at press
- Water removal (CD)
- Water removal, wet press
- Wrinkles, press section
- Show Remaining Articles (1) Collapse Articles
- Annular rings
- Baggy rolls
- Bursting or cracked rolls
- Cleaner slitting
- Corrugations
- Corrugations, winders
- Defective splices
- Dust in rolls
- Dust in the rolls
- Good roll condition, off winder
- Hard and soft spots/ridges
- Interweaving
- Loose cores
- Loose paper, in roll
- Nicked edges
- Out-of-round rolls
- Reel or roll quality
- Rewound roll quality
- Run-in of slit rolls
- Shipping roll characteristics
- Snap-offs
- Soft edges
- Starred rolls
- Telescoping
- Turned edges
- Variable density rolls
- Winder cracks
- Winding requirements
- Wrinkles, winder
- Show Remaining Articles (10) Collapse Articles
Careers
Pulp & Paper Manufacturing
- Articles coming soon
Companies
Table of Contents
1. Maintain basis weight uniformity.
— ensure that there are no “thin” areas.
2. Avoid sagging edges at couch.
— keep edges dry and with the same formation as rest of sheet.
— ensure that end seals of couch box do not leak.
3. Do not allow wrinkles in felt.
4. Crumbs tend to wrinkle the felt.
— crumbs can be scraped off outside rolls, but they must be washed off inside rolls.
5. Keep draw tight and maintain control.
— long draws can lead to wrinkles.
6. Watch for entrapment of air between felt and paper.
7. Improve the lead to press nip.
8. See that loading system for press is not jammed.