Defective splices


 

1. Be sure tape does not protrude beyond edge of sheet causing next sheet to adhere.

2. Place splicing tape about 3 mm from join to prevent bottom edge turning back.

3. Make sure iron is up to required temperature to allow for proper seal.

4. Pay particular attention when making tear-off that should be clean all the way across.

5. If splicing tape is defective, replace immediately.